🟨 When Coating Fails?

5 Causes and How to Avoid Them

Real-world examples and how to design better systems

A coating system is only as strong as its surface prep, product choice, and application method. Yet, coating failures are still common across industrial, commercial, and institutional sites β€” leading to costly repairs, downtime, and frustrated clients.

In this article, we break down the top 5 causes of coating failure, show how to recognize the warning signs, and explain how to prevent them through smart system design and proper product selection.


⚠️ 1. Poor Surface Preparation

The #1 cause of failure β€” and the most preventable.

If the surface is dirty, oily, sealed, or improperly profiled, even the best coating will fail. Lack of adhesion leads to:

How to avoid it:

β€’ Always clean, degrease, and mechanically profile the substrate (grinding, shot-blasting, etc.)
β€’ Test for moisture, pH, and contamination before applying primers or coatings


πŸ’§ 2. Moisture in the Concrete Slab

Invisible moisture = visible failure.

If a coating is applied to a slab with too much internal humidity, water vapor pressure can cause:

How to avoid it:

β€’ Always test moisture content with a calcium chloride or RH test
β€’ Use a moisture vapor barrier (MVB) like:

MAGIECHEM 975 Polyaspartic MVB for up to 5%
MAGIECHEM 5076 Epoxy MVB for up to 5%
MAGIECHEM 5087 Epoxy MVB for 5%+ or 24-hour fresh concrete


πŸ§ͺ 3. Incompatible Coating Systems

Not all coatings play well together.

Layering the wrong topcoat over a base system β€” or mixing incompatible chemistries β€” can lead to:

How to avoid it:

β€’ Always verify product compatibility between layers
β€’ Use systems tested and designed to work together
β€’ When recoating, ensure the substrate is properly sanded and compatible with the new chemistry


🌑️ 4. Improper Environmental Conditions

Temperature and humidity matter.

Applying a coating when it’s too hot, cold, humid, or windy can affect:

How to avoid it:

β€’ Respect application windows in each product’s TDS
β€’ Choose systems formulated for cold or humid conditions, such as MAGIECHEM polyaspartics that cure even at low temperatureshether you’re refreshing a worn surface, upgrading chemical resistance, or going for a decorative finish.


🎯 5. Incorrect Mixing or Application

Rushed or careless application ruins systems.

Wrong mix ratios, under-mixing, improper tools, or uneven thickness can result in:

How to avoid it:

β€’ Use a clean drill with proper paddle
β€’ Follow mixing instructions precisely
β€’ Use wet film gauges to verify thickness
β€’ Allow the product to induct if required

Always follow the MAGIECHEM Installation Guide provided with each system. If in doubt, ask our reps for clarification before starting.


🧠 Final Thoughts

Coating failures can cost you more than just materials β€” they damage your reputation.
By understanding these 5 key causes and working with the right systems, you can ensure long-lasting, high-performance results every time.

MAGIECHEM offers fully integrated, field-tested coating systems β€” supported by expert technical reps and precise product documentation.